Skip navigation
Please use this identifier to cite or link to this item: http://repositorio2.unb.br/jspui/handle/10482/33662
Files in This Item:
File SizeFormat 
ARTIGO_ExperimentalStudySolid.pdf2,8 MBAdobe PDFView/Open
Title: Experimental study of solid RC slabs strengthened on the upper surface
Análise experimental de lajes de CA reforçadas pela face superior
Authors: Campos, C. O.
Trautwein, L. M.
Gomes, R. B.
Melo, Guilherme Sales Soares de Azevedo
Assunto:: Lajes - concreto
Concreto armado
Aderência
Issue Date: 2018
Publisher: IBRACON - Instituto Brasileiro do Concreto
Citation: CAMPOS, C. O. et al. Experimental study of solid RC slabs strengthened on the upper surface. Revista IBRACON de Estruturas e Materiais, São Paulo, v. 11, n. 2, p. 255-278, abr. 2018. DOI: http://dx.doi.org/10.1590/s1983-41952018000200003. Disponível em: http://www.scielo.br/scielo.php?script=sci_arttext&pid=S1983-41952018000200255&lng=en&nrm=iso. Acesso em: 25 jan. 2019.
Abstract: Este trabalho apresenta os resultados dos ensaios de 5 lajes de concreto armado (415 cm x 415 cm x 7 cm) com o objetivo de se verificar experimentalmente a possibilidade de reforço pela face superior de lajes de concreto armado e também de se avaliar a aderência entre o concreto antigo da laje e a camada do concreto do reforço. As principais variáveis foram as deficiências da resistência do concreto e de armadura. A laje L1, de referência, foi ensaiada até a ruptura e as demais até um limite de carregamento quando foram reforçadas e reensaiadas até a ruptura. Todas as lajes romperam por flexão e nas lajes armadas com uma taxa mínima de armadura, o reforço elevou em até 30% a carga de ruptura em relação a uma laje similar sem reforço, independentemente da resistência original do concreto. Em todos os ensaios das lajes reforçadas não se detectou descolamentos ou evidências de perda de aderência entre o concreto antigo e o concreto do reforço.
Abstract: The current study presents the results of tests conducted in 5 reinforced concrete slabs (415 cm x 415 cm x 7 cm) in order to experimentally check the possibility of reinforcing their upper surface, as well as to assess the adhesion between the old and the reinforcing concrete layers in the slab. The main variables were the concrete and reinforcement strength deficiencies. Reference slab “L1” was tested until reaching the failure load, whereas the others were tested until reaching certain load limit, reinforced and retested until reaching the failure load. All slabs failed under bending. The strengthening increased the failure load by 30% in slabs reinforced at minimum reinforcement rate when they were compared to similar non-reinforced slabs, regardless of the original concrete strength. None of the tests conducted in the reinforced slabs showed detachments or evidence of adhesion loss between the old and reinforcing concretes.
DOI: http://dx.doi.org/10.1590/s1983-41952018000200003
Appears in Collections:Artigos publicados em periódicos e afins

Show full item record " class="statisticsLink btn btn-primary" href="/jspui/handle/10482/33662/statistics">



Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.